Conversions & Swaps LSX Engines in Non-LSX Vehicles
Sponsored by:
Sponsored by:

Anybody try this.."Sharkhide"

Thread Tools
 
Search this Thread
 
Old 10-04-2010, 05:37 PM
  #1  
TECH Senior Member
Thread Starter
 
Jimbo1367's Avatar
 
Join Date: Jul 2009
Posts: 7,816
Received 583 Likes on 461 Posts

Default Anybody try this.."Sharkhide"

Has anybody tried this "sharkHide" metal protectant? Its suspose to protect aluminum from oxidizing. I am thinking its perfect for all the alum. pcs. on LSx engines.

www.sharkhide.com/mpinfo.html
Old 10-04-2010, 05:58 PM
  #2  
TECH Resident
iTrader: (21)
 
Verz's Avatar
 
Join Date: Aug 2006
Location: Wichita KS
Posts: 947
Likes: 0
Received 0 Likes on 0 Posts

Default

saw that this weekend on trucks looks interesting and prolly a good investment if the price is right
Old 10-04-2010, 09:03 PM
  #3  
Launching!
 
leon phelps's Avatar
 
Join Date: Nov 2009
Location: Croydon, PA
Posts: 274
Likes: 0
Received 1 Like on 1 Post

Default

Not sure if it would work for this application. Works for pontoon boats great.

Engines get a little warmer and cool down pretty fast. Expansion and contraction would amplify the need for excellent bonding.
Old 10-05-2010, 02:30 AM
  #4  
Staging Lane
 
67firebirdak's Avatar
 
Join Date: Sep 2009
Location: Anchorage, Alaska
Posts: 71
Likes: 0
Received 0 Likes on 0 Posts
Default

Haven't tried it, but I'd be interested in seeing what the results are. If it works, could make polished aluminium look even better...
Old 10-05-2010, 05:04 AM
  #5  
On The Tree
 
turbinesurgeon's Avatar
 
Join Date: Jan 2010
Location: Fort Campbell, KY
Posts: 168
Likes: 0
Received 1 Like on 1 Post
Default

Don't think it will work on engine parts. I read the MSDS for it posted on the site, says the boiling point for the chemical is 231-270 degrees F. Here's their link...

http://www.sharkhide.com/METAL%20PROTECTANT%20MSDS.pdf
Old 10-05-2010, 07:05 PM
  #6  
Teching In
 
70texasnova's Avatar
 
Join Date: Sep 2010
Location: Gilmer, Texas
Posts: 15
Likes: 0
Received 0 Likes on 0 Posts
Default

I have a custom fabbed aluminum boat and all the surfaces inside the boat are diamond plate that have been sandblasted to give it a rough, sandpaper feel. It looks cool, but it stains really easy, so I tried the Sharkhide after reading about it in Carcraft or Hotrod or one of those magazines. Its worked out really good so far and it didn't change the texture or appearance of any of the surfaces I've put it on.

Before I ordered it, I called the company on the phone and asked a lot of questions. They were really helpful and have used it in a lot of applications, so they could probably tell you really easily if it would be right for under the hood or high-heat use.

Use it outside though, its about the strongest smelling stuff I've applied in a long time.

Last edited by 70texasnova; 10-05-2010 at 07:07 PM. Reason: Forgot something
Old 10-05-2010, 07:47 PM
  #7  
Teching In
 
A-Body's Avatar
 
Join Date: Nov 2008
Posts: 21
Likes: 0
Received 0 Likes on 0 Posts
Default

Always been a fan of glass bead blasting aluminum parts such as acc. brackets, intakes, trans cases and such... Looks good when done and when it starts to get a little oily hit with degreaser and wash...looks like new. Take it to a monument (TOMB STONE) maker near you and ask how much. The ppl. do glass beading all day and know not to stay in one area too long. I know its not sharkhide but just my .02
Old 07-25-2012, 05:00 PM
  #8  
On The Tree
iTrader: (1)
 
Vexzer's Avatar
 
Join Date: Apr 2007
Location: Castle Hills, TX
Posts: 198
Received 0 Likes on 0 Posts

Default

Reviving an old thread.
"SharkHideŽ is the ideal long-term protectant for steel, aluminum, copper, brass, stainless and fiberglass"

Just saw this on "Gearz" or "Trucks" TV show this week. Never heard of it. This thread since 2010. What's the Jury say about the stuff for long term and steel/aluminum use?
Old 07-25-2012, 07:20 PM
  #9  
TECH Enthusiast
iTrader: (3)
 
rotor vs. piston's Avatar
 
Join Date: Jan 2004
Posts: 583
Likes: 0
Received 2 Likes on 2 Posts

Default

Another forum, but interesting comments

http://www.thehulltruth.com/boating-...otector.html#b
Old 07-25-2012, 09:04 PM
  #10  
Staging Lane
 
ealvarez11's Avatar
 
Join Date: Mar 2010
Posts: 60
Received 5 Likes on 4 Posts

Default

fyi aluminum is not prone to oxidation...staining yes but not oxidation (i.e. rust)
Old 07-25-2012, 09:22 PM
  #11  
TECH Apprentice
 
Krom's Avatar
 
Join Date: Sep 2006
Posts: 328
Received 2 Likes on 2 Posts

Default

Originally Posted by ealvarez11
fyi aluminum is not prone to oxidation...staining yes but not oxidation (i.e. rust)
It sure is, it just turns chalky white, instead of red
Old 07-26-2012, 09:38 AM
  #12  
On The Tree
iTrader: (1)
 
Vexzer's Avatar
 
Join Date: Apr 2007
Location: Castle Hills, TX
Posts: 198
Received 0 Likes on 0 Posts

Default

Originally Posted by rotor vs. piston
Another forum, but interesting comments

http://www.thehulltruth.com/boating-...otector.html#b
Thanks for the comments!



Quick Reply: Anybody try this.."Sharkhide"